Why Pad Heads Crack Tear Strength and HY-912 Long Life Advantage

2026,10,28
The Cracking Problem Pad heads bend between the steel plate and product thousands of times daily. Silicone with low tear strength develops surface micro cracks that grow until the head fails.
default name

Tear Strength Matters Tear strength in kN per m resists crack growth. HY-912 reaches 25kN per m, highest among 30 Shore A models, versus 22 for HY-901 and 24 for HY-902.

HY-912 Advantage Optimized formula keeps 30A and 4.0MPa tensile while boosting tear. The 340 percent elongation suits flat printing. Customer feedback shows over 30 percent more prints per pad.

Selection Long running lines choose HY-912. Moderate detail work choose HY-902. Budget simple jobs choose HY-901.

Contact Us

Author:

Ms. zhou

E-mail:

alice@szrl.net

Phone/WhatsApp:

+86 18938861889

Popular Products
You may also like
Related Categories

Email to this supplier

Subject:
Email:
Message:

Your message must be between 20-8000 characters

  • Send Inquiry

Copyright © 2026 Shenzhen Hong Ye Jie Technology Co., Ltd All rights reserved. Privacy Policy

We will contact you immediately

Fill in more information so that we can get in touch with you faster

Privacy statement: Your privacy is very important to Us. Our company promises not to disclose your personal information to any external company with out your explicit permission.

Send