Product Overview
Understanding why HONG YE SILICONE liquid silicone foam behaves the way it does makes specification, processing and troubleshooting far easier. The product is a two-component addition-curing silicone rubber: Part A typically carries the platinum catalyst and vinyl-functional polysiloxane, while Part B carries the cross-linker and the foaming component. When the two are combined at a 1:1 ratio, two reactions run at the same time. The addition reaction links vinyl groups to silicon-hydrogen bonds and builds the elastomeric network, while the foaming reaction releases gas inside that network and expands it into millions of closed cells. Because gelling and expansion progress together at a rate set by the formulation and the temperature, the mix foams evenly wherever it sits, whether in a 1 mm sheet or a 50 mm pad. The result is a white, uniform, closed-cell Silicone Foam of 2×–7× expansion, density 0.15–0.525 g/cm³ and Shore C hardness 2–35, which keeps its elasticity from -65℃ to 200℃ and carries a UL94 V-0 flame rating. That chemistry, rather than any additive, explains the foam's low shrinkage, absence of odor, lack of migration and stable long-term rebound.
Technical Specifications
Cure mechanism: platinum-catalyzed addition (hydrosilylation) cross-linking.
Foaming mechanism: gas released within the curing network, forming closed cells.
Mix ratio: 1:1 by weight.
Foaming ratio: 2× to 7× original volume.
Cured density: approximately 0.15–0.525 g/cm³.
Hardness: Shore C 2–35.
Cell type: closed-cell, uniform distribution.
Working time: roughly 2–3 minutes after mixing, temperature dependent.
Service temperature: -65℃ to 200℃ long term.
Linear shrinkage: low, stable dimensions after cure.
Flame rating: UL94 V-0.
Chemical character: inert, non-toxic, non-corrosive, odor-free, no radioactivity.
Cured color: white as standard.
Packaging: Part A 25/200/250 kg, Part B 20/25/200 kg.
Transport and storage: non-dangerous goods; sealed, cool, dry, away from sunlight and heat.
Shelf life: 12 months in unopened containers.
Product Images and Videos
Useful page assets include a simple diagram of the two-part mix entering the mold and rising, macro photographs of the closed-cell structure at two expansion levels, a comparison of foam cross-sections cut from thin and thick parts to show even cell size, and a short clip of the mix gelling while it expands. Visuals of cell walls help buyers understand why the foam resists water and why it does not collapse under repeated compression.
Product Features
Even Expansion in Any Thickness: because gel and gas generation advance together, cell growth is governed by chemistry rather than by heat penetrating from the mold surface, so thick and thin parts foam alike.
Closed-Cell Barrier Structure: sealed cell walls limit water ingress, block dust and reduce thermal convection, which is why the foam suits sealing and insulation duties.
No Blowing Agent Residue: gas is generated inside the reacting network rather than added as a physical agent, so there is no residual solvent, no odor and no post-cure outgassing.
Low Shrinkage and Stable Dimensions: cross-linking sets the shape before expansion finishes settling, giving low linear shrinkage and predictable part dimensions.
No Migration or Embrittlement: an addition-cured silicone network contains no plasticizer to migrate, so the foam stays soft and does not harden or stain adjacent materials.
Intrinsic Temperature and Flame Behavior: the silicone backbone, not an additive package, provides -65℃ to 200℃ service and UL94 V-0 performance, so properties do not wash out with age.
How to Use
Step 1 – Understand the Two Reactions: recognize that cure and foaming compete for the same working time, so any delay after mixing reduces expansion.
Step 2 – Stir Both Components: stir A and B separately so catalyst and cross-linker are evenly distributed before weighing.
Step 3 – Mix at 1:1 Thoroughly: incomplete mixing leaves platinum-poor regions that cure slowly and foam unevenly.
Step 4 – Degas the Mix: remove air entrained during stirring, since trapped air adds macro voids on top of the intended cell structure.
Step 5 – Control the Temperature: keep drums, room and mold within the recommended window, because cold slows both reactions and heat accelerates them unevenly.
Step 6 – Avoid Contamination: sulfur, tin, amine, phosphorus and certain plasticizers poison the platinum catalyst and stop or slow cure.
Application Scenarios
Sealing gaskets and rings that rely on closed cells to block water and dust; cushioning pads and insoles that rely on uniform cell size for consistent feel; insulation layers that rely on still air in closed cells; filler for Human Body Silicone and robot silicone parts that relies on light weight without odor; and precision parts where low shrinkage and stable dimensions matter.
Value for Buyers
A chemistry-driven process means fewer rejects from thickness variation, no odor complaints from end users, no staining of adjacent materials, and predictable dimensions that simplify assembly; because the same mechanism serves every grade in the range, buyers get consistent behavior from 2× to 7× and can standardize on one supplier.
Certifications and Compliance
Manufactured under ISO 9001 quality management, CE Certification and the EU RoHS Directive, with a UL94 V-0 flame rating; material data sheets, batch records and test reports support regulatory review.
Customization Options
Expansion ratio, density, hardness, color, viscosity, cure speed and working time can be adjusted by reformulating the two components; matched A/B sets, trial drums and process guidance are provided for validation.
Production Process and Quality Control
We follow a five-step routine: raw material screening, precision automated mixing, performance testing of density, hardness, flame rating and compression set, curing and dimension verification, and sealed packaging, on 20 production lines with stable export supply.
FAQ
Q: Why does the foam not depend on part thickness?
A: Because cure and gas generation are chemical and run together throughout the mix, rather than relying on heat reaching the center of a thick part.
Q: Why is the foam closed-cell?
A: Gas is released inside the gelling network before the walls fully set, so cells stay sealed instead of rupturing into open channels.
Q: Why is there no smell?
A: The material contains no solvent or physical blowing agent; the gas comes from the reaction itself, leaving no residue to evaporate.